Aluminum-silicon casting alloys : an atlas of microfractographs

Author: Małgorzata Warmuzek
Publisher: Materials Park, OH : ASM International, 2004.
Edition/Format:   eBook : Document : EnglishView all editions and formats
Summary:
This atlas provides an in-depth understanding of the metallurgy and fracture behavior of aluminum-silicon casting alloys, which are used in a wide variety of automotive, aerospace, and consumer product applications. The atlas includes over 300 high-definition microfractographs of fracture profiles and fracture surfaces, accompanied with detailed descriptions and analysis of the fracture features and their  Read more...
Rating:

(not yet rated) 0 with reviews - Be the first.

Subjects
More like this

 

Find a copy in the library

&AllPage.SpinnerRetrieving; Finding libraries that hold this item...

Details

Genre/Form: Electronic books
Scientific atlases
Atlases
Additional Physical Format: Print version:
Warmuzek, Małgorzata.
Aluminum-silicon casting alloys.
Materials Park, OH : ASM International, 2004
(DLC) 2004040998
(OCoLC)54024176
Material Type: Document, Internet resource
Document Type: Internet Resource, Computer File
All Authors / Contributors: Małgorzata Warmuzek
ISBN: 9781615030750 1615030751
OCLC Number: 300532760
Reproduction Notes: Electronic reproduction. [S.l.] : HathiTrust Digital Library, 2010. MiAaHDL
Description: 1 online resource (v, 124 pages) : illustrations
Details: Master and use copy. Digital master created according to Benchmark for Faithful Digital Reproductions of Monographs and Serials, Version 1. Digital Library Federation, December 2002.
Contents: About the Author --
Preface --
Introduction to aluminum-silicon casting alloys --
Fractography --
Microstructural aspects of the failure of aluminum-silicon casting alloys --
Alloy 336.0 (AlSi13Mg1CuNi) --
Alloy 355.0 (AlSi5Cu) --
Alloy 356.0 (AlSi7Mg) --
Alloy 359.0 (AlSi9Mg) --
Alloy 390.0 (AlSi21CuNi) --
Alloy 413.0 (AlSi11) --
Material defects on fracture surfaces.
Responsibility: Małgorzata Warmuzek.
More information:

Abstract:

Provides an in-depth understanding of the metallurgy and fracture behaviour of aluminum-silicon casting alloys, which are used in a wide variety of automotive, aerospace, and consumer product  Read more...

Reviews

User-contributed reviews
Retrieving GoodReads reviews...
Retrieving DOGObooks reviews...

Tags

Be the first.
Confirm this request

You may have already requested this item. Please select Ok if you would like to proceed with this request anyway.

Linked Data


Primary Entity

<http://www.worldcat.org/oclc/300532760> # Aluminum-silicon casting alloys : an atlas of microfractographs
    a schema:CreativeWork, schema:MediaObject, schema:Book ;
    library:oclcnum "300532760" ;
    library:placeOfPublication <http://experiment.worldcat.org/entity/work/data/864878011#Place/materials_park_oh> ; # Materials Park, OH
    library:placeOfPublication <http://id.loc.gov/vocabulary/countries/ohu> ;
    schema:about <http://id.worldcat.org/fast/806322> ; # Aluminum alloys--Fracture
    schema:about <http://experiment.worldcat.org/entity/work/data/864878011#Topic/technology_&_engineering_metallurgy> ; # TECHNOLOGY & ENGINEERING--Metallurgy
    schema:about <http://dewey.info/class/669.722/e22/> ;
    schema:about <http://id.worldcat.org/fast/806326> ; # Aluminum alloys--Metallography
    schema:about <http://id.loc.gov/authorities/subjects/sh85003980> ; # Aluminum alloys--Fracture
    schema:about <http://id.loc.gov/authorities/subjects/sh85003983> ; # Aluminum alloys--Metallography
    schema:bookFormat schema:EBook ;
    schema:creator <http://viaf.org/viaf/163391215> ; # Małgorzata Warmuzek
    schema:datePublished "2004" ;
    schema:description "About the Author -- Preface -- Introduction to aluminum-silicon casting alloys -- Fractography -- Microstructural aspects of the failure of aluminum-silicon casting alloys -- Alloy 336.0 (AlSi13Mg1CuNi) -- Alloy 355.0 (AlSi5Cu) -- Alloy 356.0 (AlSi7Mg) -- Alloy 359.0 (AlSi9Mg) -- Alloy 390.0 (AlSi21CuNi) -- Alloy 413.0 (AlSi11) -- Material defects on fracture surfaces."@en ;
    schema:description "This atlas provides an in-depth understanding of the metallurgy and fracture behavior of aluminum-silicon casting alloys, which are used in a wide variety of automotive, aerospace, and consumer product applications. The atlas includes over 300 high-definition microfractographs of fracture profiles and fracture surfaces, accompanied with detailed descriptions and analysis of the fracture features and their significance in the selection, processing, properties, and performance of the alloy. The microfractographs are described and classified according to criteria described in detail in the introductory chapters in the book. The factors determining the fracture mechanism in these alloys, on the basis of their physical and mechanical properties and fracture mechanics, are described and analyzed. The set of micrographs in this atlas include several unique features: classification according to the alloy and its processing history, detailed analysis of selected microregions of the fracture surface, reference of the fracture features to the phase constituents of the alloy, and high resolution and high microscopic magnification of the SEM images. This book will be of great value to anyone involved in the selection, processing, application, testing, or evaluation of aluminum-silicon castings. The target audience includes metallurgists, foundry personnel, failure analysts, purchasers of castings, researchers in physical and mechanical metallurgy, students, and educators."@en ;
    schema:exampleOfWork <http://worldcat.org/entity/work/id/864878011> ;
    schema:genre "Scientific atlases"@en ;
    schema:genre "Electronic books"@en ;
    schema:inLanguage "en" ;
    schema:isSimilarTo <http://www.worldcat.org/oclc/54024176> ;
    schema:name "Aluminum-silicon casting alloys : an atlas of microfractographs"@en ;
    schema:productID "300532760" ;
    schema:publication <http://www.worldcat.org/title/-/oclc/300532760#PublicationEvent/materials_park_oh_asm_international_2004> ;
    schema:publisher <http://experiment.worldcat.org/entity/work/data/864878011#Agent/asm_international> ; # ASM International
    schema:url <http://books.google.com/books?id=G8RTAAAAMAAJ> ;
    schema:url <http://public.eblib.com/choice/publicfullrecord.aspx?p=3002394> ;
    schema:url <http://catdir.loc.gov/catdir/toc/fy045/2004040998.html> ;
    schema:url <http://www.books24x7.com/marc.asp?bookid=42624> ;
    schema:url <http://er.llcc.edu:2048/login?url=http://search.ebscohost.com/login.aspx?direct=true&scope=site&db=nlebk&AN=395866> ;
    schema:url <http://site.ebrary.com/id/10320387> ;
    schema:url <http://search.ebscohost.com/login.aspx?direct=true&scope=site&db=nlebk&db=nlabk&AN=395866> ;
    schema:url <http://ebookcentral.proquest.com/lib/warw/detail.action?docID=3002394> ;
    schema:url <http://ebookcentral.proquest.com/lib/columbia/detail.action?docID=3002394> ;
    schema:url <http://catalog.hathitrust.org/api/volumes/oclc/54024176.html> ;
    schema:url <http://public.ebookcentral.proquest.com/choice/publicfullrecord.aspx?p=3002394> ;
    schema:workExample <http://worldcat.org/isbn/9781615030750> ;
    wdrs:describedby <http://www.worldcat.org/title/-/oclc/300532760> ;
    .


Related Entities

<http://experiment.worldcat.org/entity/work/data/864878011#Agent/asm_international> # ASM International
    a bgn:Agent ;
    schema:name "ASM International" ;
    .

<http://experiment.worldcat.org/entity/work/data/864878011#Place/materials_park_oh> # Materials Park, OH
    a schema:Place ;
    schema:name "Materials Park, OH" ;
    .

<http://experiment.worldcat.org/entity/work/data/864878011#Topic/technology_&_engineering_metallurgy> # TECHNOLOGY & ENGINEERING--Metallurgy
    a schema:Intangible ;
    schema:name "TECHNOLOGY & ENGINEERING--Metallurgy"@en ;
    .

<http://id.loc.gov/authorities/subjects/sh85003980> # Aluminum alloys--Fracture
    a schema:Intangible ;
    schema:name "Aluminum alloys--Fracture"@en ;
    .

<http://id.loc.gov/authorities/subjects/sh85003983> # Aluminum alloys--Metallography
    a schema:Intangible ;
    schema:name "Aluminum alloys--Metallography"@en ;
    .

<http://id.worldcat.org/fast/806322> # Aluminum alloys--Fracture
    a schema:Intangible ;
    schema:name "Aluminum alloys--Fracture"@en ;
    .

<http://id.worldcat.org/fast/806326> # Aluminum alloys--Metallography
    a schema:Intangible ;
    schema:name "Aluminum alloys--Metallography"@en ;
    .

<http://viaf.org/viaf/163391215> # Małgorzata Warmuzek
    a schema:Person ;
    schema:familyName "Warmuzek" ;
    schema:givenName "Małgorzata" ;
    schema:name "Małgorzata Warmuzek" ;
    .

<http://worldcat.org/isbn/9781615030750>
    a schema:ProductModel ;
    schema:isbn "1615030751" ;
    schema:isbn "9781615030750" ;
    .

<http://www.worldcat.org/oclc/54024176>
    a schema:CreativeWork ;
    rdfs:label "Aluminum-silicon casting alloys." ;
    schema:description "Print version:" ;
    schema:isSimilarTo <http://www.worldcat.org/oclc/300532760> ; # Aluminum-silicon casting alloys : an atlas of microfractographs
    .


Content-negotiable representations

Close Window

Please sign in to WorldCat 

Don't have an account? You can easily create a free account.