Assessment of the stress corrosion cracking of post-tensioned tendons at the John Day Lock Preview this item
ClosePreview this item
Checking...

Assessment of the stress corrosion cracking of post-tensioned tendons at the John Day Lock

Author: E G Segan; D Socie; D Morrow; Construction Engineering Research Laboratory (U.S. : 1969-1992)
Publisher: Champaign, Ill. : US Army Corps of Engineers, Construction Engineering Research Laboratory ; [Springfield, Va.] : [Available from National Technical Information Service], [1984]
Series: Technical report (Construction Engineering Research Laboratory (U.S. : 1969-1992)), M-349.
Edition/Format:   Print book : National government publication : EnglishView all editions and formats
Rating:

(not yet rated) 0 with reviews - Be the first.

Subjects
More like this

Find a copy in the library

&AllPage.SpinnerRetrieving; Finding libraries that hold this item...

Details

Material Type: Government publication, National government publication
Document Type: Book
All Authors / Contributors: E G Segan; D Socie; D Morrow; Construction Engineering Research Laboratory (U.S. : 1969-1992)
OCLC Number: 11115505
Notes: Cover title.
"June 1984."
Description: 26 pages : illustrations ; 28 cm.
Series Title: Technical report (Construction Engineering Research Laboratory (U.S. : 1969-1992)), M-349.
Responsibility: by E.G. Segan, D. Socie, D. Morrow.

Reviews

User-contributed reviews
Retrieving GoodReads reviews...
Retrieving DOGObooks reviews...

Tags

Be the first.
Confirm this request

You may have already requested this item. Please select Ok if you would like to proceed with this request anyway.

Linked Data


Primary Entity

<http://www.worldcat.org/oclc/11115505> # Assessment of the stress corrosion cracking of post-tensioned tendons at the John Day Lock
    a schema:CreativeWork, schema:Book ;
   library:oclcnum "11115505" ;
   library:placeOfPublication <http://experiment.worldcat.org/entity/work/data/3884606#Place/springfield_va> ; # Springfield, Va.
   library:placeOfPublication <http://experiment.worldcat.org/entity/work/data/3884606#Place/champaign_ill> ; # Champaign, Ill.
   library:placeOfPublication <http://id.loc.gov/vocabulary/countries/ilu> ;
   schema:about <http://dewey.info/class/623/> ;
   schema:about <http://id.worldcat.org/fast/1001691> ; # Locks (Hydraulic engineering)
   schema:about <http://experiment.worldcat.org/entity/work/data/3884606#Place/john_day_lock_or_and_wash> ; # John Day Lock (Or. and Wash.)
   schema:about <http://id.worldcat.org/fast/1134948> ; # Stress corrosion
   schema:bookFormat bgn:PrintBook ;
   schema:contributor <http://viaf.org/viaf/55717049> ; # D. Socie
   schema:contributor <http://viaf.org/viaf/124258450> ; # Construction Engineering Research Laboratory (U.S. : 1969-1992)
   schema:contributor <http://viaf.org/viaf/159836768> ; # D. Morrow
   schema:creator <http://viaf.org/viaf/40728128> ; # Ellen G. Segan
   schema:datePublished "1984" ;
   schema:exampleOfWork <http://worldcat.org/entity/work/id/3884606> ;
   schema:genre "Government publication"@en ;
   schema:genre "National government publication"@en ;
   schema:inLanguage "en" ;
   schema:isPartOf <http://experiment.worldcat.org/entity/work/data/3884606#Series/technical_report_construction_engineering_research_laboratory_u_s_1969_1992> ; # Technical report (Construction Engineering Research Laboratory (U.S. : 1969-1992)) ;
   schema:isPartOf <http://experiment.worldcat.org/entity/work/data/3884606#Series/cerl_technical_report> ; # CERL technical report ;
   schema:name "Assessment of the stress corrosion cracking of post-tensioned tendons at the John Day Lock"@en ;
   schema:productID "11115505" ;
   schema:publication <http://www.worldcat.org/title/-/oclc/11115505#PublicationEvent/champaign_ill_us_army_corps_of_engineers_construction_engineering_research_laboratory_springfield_va_available_from_national_technical_information_service_1984> ;
   schema:publisher <http://experiment.worldcat.org/entity/work/data/3884606#Agent/available_from_national_technical_information_service> ; # [Available from National Technical Information Service]
   schema:publisher <http://experiment.worldcat.org/entity/work/data/3884606#Agent/us_army_corps_of_engineers_construction_engineering_research_laboratory> ; # US Army Corps of Engineers, Construction Engineering Research Laboratory
   wdrs:describedby <http://www.worldcat.org/title/-/oclc/11115505> ;
    .


Related Entities

<http://experiment.worldcat.org/entity/work/data/3884606#Agent/available_from_national_technical_information_service> # [Available from National Technical Information Service]
    a bgn:Agent ;
   schema:name "[Available from National Technical Information Service]" ;
    .

<http://experiment.worldcat.org/entity/work/data/3884606#Agent/us_army_corps_of_engineers_construction_engineering_research_laboratory> # US Army Corps of Engineers, Construction Engineering Research Laboratory
    a bgn:Agent ;
   schema:name "US Army Corps of Engineers, Construction Engineering Research Laboratory" ;
    .

<http://experiment.worldcat.org/entity/work/data/3884606#Place/champaign_ill> # Champaign, Ill.
    a schema:Place ;
   schema:name "Champaign, Ill." ;
    .

<http://experiment.worldcat.org/entity/work/data/3884606#Place/john_day_lock_or_and_wash> # John Day Lock (Or. and Wash.)
    a schema:Place ;
   schema:name "John Day Lock (Or. and Wash.)" ;
    .

<http://experiment.worldcat.org/entity/work/data/3884606#Place/springfield_va> # Springfield, Va.
    a schema:Place ;
   schema:name "Springfield, Va." ;
    .

<http://experiment.worldcat.org/entity/work/data/3884606#Series/cerl_technical_report> # CERL technical report ;
    a bgn:PublicationSeries ;
   schema:hasPart <http://www.worldcat.org/oclc/11115505> ; # Assessment of the stress corrosion cracking of post-tensioned tendons at the John Day Lock
   schema:name "CERL technical report ;" ;
    .

<http://experiment.worldcat.org/entity/work/data/3884606#Series/technical_report_construction_engineering_research_laboratory_u_s_1969_1992> # Technical report (Construction Engineering Research Laboratory (U.S. : 1969-1992)) ;
    a bgn:PublicationSeries ;
   schema:hasPart <http://www.worldcat.org/oclc/11115505> ; # Assessment of the stress corrosion cracking of post-tensioned tendons at the John Day Lock
   schema:name "Technical report (Construction Engineering Research Laboratory (U.S. : 1969-1992)) ;" ;
    .

<http://id.worldcat.org/fast/1001691> # Locks (Hydraulic engineering)
    a schema:Intangible ;
   schema:name "Locks (Hydraulic engineering)"@en ;
    .

<http://id.worldcat.org/fast/1134948> # Stress corrosion
    a schema:Intangible ;
   schema:name "Stress corrosion"@en ;
    .

<http://viaf.org/viaf/124258450> # Construction Engineering Research Laboratory (U.S. : 1969-1992)
    a schema:Organization ;
   schema:name "Construction Engineering Research Laboratory (U.S. : 1969-1992)" ;
    .

<http://viaf.org/viaf/159836768> # D. Morrow
    a schema:Person ;
   schema:familyName "Morrow" ;
   schema:givenName "D." ;
   schema:name "D. Morrow" ;
    .

<http://viaf.org/viaf/40728128> # Ellen G. Segan
    a schema:Person ;
   schema:familyName "Segan" ;
   schema:givenName "Ellen G." ;
   schema:givenName "E. G." ;
   schema:name "Ellen G. Segan" ;
    .

<http://viaf.org/viaf/55717049> # D. Socie
    a schema:Person ;
   schema:familyName "Socie" ;
   schema:givenName "D." ;
   schema:name "D. Socie" ;
    .

<http://www.worldcat.org/title/-/oclc/11115505>
    a genont:InformationResource, genont:ContentTypeGenericResource ;
   schema:about <http://www.worldcat.org/oclc/11115505> ; # Assessment of the stress corrosion cracking of post-tensioned tendons at the John Day Lock
   schema:dateModified "2018-11-11" ;
   void:inDataset <http://purl.oclc.org/dataset/WorldCat> ;
    .

<http://www.worldcat.org/title/-/oclc/11115505#PublicationEvent/champaign_ill_us_army_corps_of_engineers_construction_engineering_research_laboratory_springfield_va_available_from_national_technical_information_service_1984>
    a schema:PublicationEvent ;
   schema:location <http://experiment.worldcat.org/entity/work/data/3884606#Place/springfield_va> ; # Springfield, Va.
   schema:location <http://experiment.worldcat.org/entity/work/data/3884606#Place/champaign_ill> ; # Champaign, Ill.
   schema:organizer <http://experiment.worldcat.org/entity/work/data/3884606#Agent/available_from_national_technical_information_service> ; # [Available from National Technical Information Service]
   schema:organizer <http://experiment.worldcat.org/entity/work/data/3884606#Agent/us_army_corps_of_engineers_construction_engineering_research_laboratory> ; # US Army Corps of Engineers, Construction Engineering Research Laboratory
   schema:startDate "1984" ;
    .


Content-negotiable representations

Close Window

Please sign in to WorldCat 

Don't have an account? You can easily create a free account.