skip to content
Covid-19 virus
COVID-19 Resources

Reliable information about the coronavirus (COVID-19) is available from the World Health Organization (current situation, international travel). Numerous and frequently-updated resource results are available from this WorldCat.org search. OCLC’s WebJunction has pulled together information and resources to assist library staff as they consider how to handle coronavirus issues in their communities.

Image provided by: CDC/ Alissa Eckert, MS; Dan Higgins, MAM
Fabrication development for ODS-superalloy, air-cooled turbine blades : final report Preview this item
ClosePreview this item
Checking...

Fabrication development for ODS-superalloy, air-cooled turbine blades : final report

Author: D J Moracz; Lewis Research Center.; TRW Inc. Materials and Manufacturing Technology Center.
Publisher: [Cleveland, Ohio?] : National Aeronautics and Space Administration, NASA Lewis Research Center ; [Springfield, Va.] : [For sale by the National Technical Information Service], [1984]
Series: NASA contractor report, 174650.
Edition/Format:   Book   Microform : National government publication : Microfiche : English
Rating:

(not yet rated) 0 with reviews - Be the first.

Subjects
More like this

Find a copy in the library

&AllPage.SpinnerRetrieving; Finding libraries that hold this item...

Details

Material Type: Government publication, National government publication
Document Type: Book
All Authors / Contributors: D J Moracz; Lewis Research Center.; TRW Inc. Materials and Manufacturing Technology Center.
OCLC Number: 11674423
Notes: "TRW Inc., Materials and Manufacturing Technology Center."
"January 1984."
"N84-25711"--Microfiche header.
Reproduction Notes: Microfiche. [Washington, D.C.? : National Aeronautics and Space Administration, 1984]. 2 microfiches.
Description: 1 volume : illustrations ; 28 cm.
Series Title: NASA contractor report, 174650.
Other Titles: Fabrication development for O.D.S.-superalloy, air-cooled turbine blades
Responsibility: D.J. Moracz.

Reviews

User-contributed reviews
Retrieving GoodReads reviews...
Retrieving DOGObooks reviews...

Tags

Be the first.

Similar Items

Confirm this request

You may have already requested this item. Please select Ok if you would like to proceed with this request anyway.

Linked Data


Primary Entity<\/h3>
<http:\/\/www.worldcat.org\/oclc\/11674423<\/a>> # Fabrication development for ODS-superalloy, air-cooled turbine blades : final report<\/span>\u00A0\u00A0\u00A0\u00A0a bgn:Microform<\/a>, schema:CreativeWork<\/a>, schema:Book<\/a> ;\u00A0\u00A0\u00A0library:oclcnum<\/a> \"11674423<\/span>\" ;\u00A0\u00A0\u00A0library:placeOfPublication<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Place\/springfield_va<\/a>> ; # Springfield, Va.<\/span>\u00A0\u00A0\u00A0library:placeOfPublication<\/a> <http:\/\/id.loc.gov\/vocabulary\/countries\/ohu<\/a>> ;\u00A0\u00A0\u00A0library:placeOfPublication<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Place\/cleveland_ohio<\/a>> ; # Cleveland, Ohio?<\/span>\u00A0\u00A0\u00A0schema:about<\/a> <http:\/\/id.loc.gov\/authorities\/subjects\/sh85003724<\/a>> ; # Alloys--Testing<\/span>\u00A0\u00A0\u00A0schema:about<\/a> <http:\/\/id.worldcat.org\/fast\/805742<\/a>> ; # Alloys--Testing<\/span>\u00A0\u00A0\u00A0schema:about<\/a> <http:\/\/id.worldcat.org\/fast\/1159117<\/a>> ; # Turbines--Blades<\/span>\u00A0\u00A0\u00A0schema:about<\/a> <http:\/\/id.loc.gov\/authorities\/subjects\/sh85138720<\/a>> ; # Turbines--Blades<\/span>\u00A0\u00A0\u00A0schema:alternateName<\/a> \"Fabrication development for O.D.S.-superalloy, air-cooled turbine blades<\/span>\" ;\u00A0\u00A0\u00A0schema:contributor<\/a> <http:\/\/viaf.org\/viaf\/155061179<\/a>> ; # Lewis Research Center.<\/span>\u00A0\u00A0\u00A0schema:contributor<\/a> <http:\/\/viaf.org\/viaf\/125539729<\/a>> ; # TRW Inc. Materials and Manufacturing Technology Center.<\/span>\u00A0\u00A0\u00A0schema:creator<\/a> <http:\/\/viaf.org\/viaf\/23544921<\/a>> ; # Donald J. Moracz<\/span>\u00A0\u00A0\u00A0schema:datePublished<\/a> \"1984<\/span>\" ;\u00A0\u00A0\u00A0schema:exampleOfWork<\/a> <http:\/\/worldcat.org\/entity\/work\/id\/4482037<\/a>> ;\u00A0\u00A0\u00A0schema:genre<\/a> \"Government publication<\/span>\"@en<\/a> ;\u00A0\u00A0\u00A0schema:genre<\/a> \"National government publication<\/span>\"@en<\/a> ;\u00A0\u00A0\u00A0schema:inLanguage<\/a> \"en<\/span>\" ;\u00A0\u00A0\u00A0schema:isPartOf<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Series\/nasa_cr<\/a>> ; # NASA CR ;<\/span>\u00A0\u00A0\u00A0schema:isPartOf<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Series\/nasa_contractor_report<\/a>> ; # NASA contractor report ;<\/span>\u00A0\u00A0\u00A0schema:name<\/a> \"Fabrication development for ODS-superalloy, air-cooled turbine blades : final report<\/span>\"@en<\/a> ;\u00A0\u00A0\u00A0schema:productID<\/a> \"11674423<\/span>\" ;\u00A0\u00A0\u00A0schema:publication<\/a> <http:\/\/www.worldcat.org\/title\/-\/oclc\/11674423#PublicationEvent\/cleveland_ohio_national_aeronautics_and_space_administration_nasa_lewis_research_center_springfield_va_for_sale_by_the_national_technical_information_service_1984<\/a>> ;\u00A0\u00A0\u00A0schema:publisher<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Agent\/for_sale_by_the_national_technical_information_service<\/a>> ; # [For sale by the National Technical Information Service]<\/span>\u00A0\u00A0\u00A0schema:publisher<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Agent\/national_aeronautics_and_space_administration_nasa_lewis_research_center<\/a>> ; # National Aeronautics and Space Administration, NASA Lewis Research Center<\/span>\u00A0\u00A0\u00A0wdrs:describedby<\/a> <http:\/\/www.worldcat.org\/title\/-\/oclc\/11674423<\/a>> ;\u00A0\u00A0\u00A0\u00A0.<\/div>

Related Entities<\/h3>
<http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Agent\/for_sale_by_the_national_technical_information_service<\/a>> # [For sale by the National Technical Information Service]<\/span>\u00A0\u00A0\u00A0\u00A0a bgn:Agent<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"[For sale by the National Technical Information Service]<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Agent\/national_aeronautics_and_space_administration_nasa_lewis_research_center<\/a>> # National Aeronautics and Space Administration, NASA Lewis Research Center<\/span>\u00A0\u00A0\u00A0\u00A0a bgn:Agent<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"National Aeronautics and Space Administration, NASA Lewis Research Center<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Place\/cleveland_ohio<\/a>> # Cleveland, Ohio?<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Place<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"Cleveland, Ohio?<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Place\/springfield_va<\/a>> # Springfield, Va.<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Place<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"Springfield, Va.<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Series\/nasa_contractor_report<\/a>> # NASA contractor report ;<\/span>\u00A0\u00A0\u00A0\u00A0a bgn:PublicationSeries<\/a> ;\u00A0\u00A0\u00A0schema:hasPart<\/a> <http:\/\/www.worldcat.org\/oclc\/11674423<\/a>> ; # Fabrication development for ODS-superalloy, air-cooled turbine blades : final report<\/span>\u00A0\u00A0\u00A0schema:name<\/a> \"NASA contractor report ;<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Series\/nasa_cr<\/a>> # NASA CR ;<\/span>\u00A0\u00A0\u00A0\u00A0a bgn:PublicationSeries<\/a> ;\u00A0\u00A0\u00A0schema:hasPart<\/a> <http:\/\/www.worldcat.org\/oclc\/11674423<\/a>> ; # Fabrication development for ODS-superalloy, air-cooled turbine blades : final report<\/span>\u00A0\u00A0\u00A0schema:name<\/a> \"NASA CR ;<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/id.loc.gov\/authorities\/subjects\/sh85003724<\/a>> # Alloys--Testing<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Intangible<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"Alloys--Testing<\/span>\"@en<\/a> ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/id.loc.gov\/authorities\/subjects\/sh85138720<\/a>> # Turbines--Blades<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Intangible<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"Turbines--Blades<\/span>\"@en<\/a> ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/id.loc.gov\/vocabulary\/countries\/ohu<\/a>>\u00A0\u00A0\u00A0\u00A0a schema:Place<\/a> ;\u00A0\u00A0\u00A0dcterms:identifier<\/a> \"ohu<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/id.worldcat.org\/fast\/1159117<\/a>> # Turbines--Blades<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Intangible<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"Turbines--Blades<\/span>\"@en<\/a> ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/id.worldcat.org\/fast\/805742<\/a>> # Alloys--Testing<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Intangible<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"Alloys--Testing<\/span>\"@en<\/a> ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/viaf.org\/viaf\/125539729<\/a>> # TRW Inc. Materials and Manufacturing Technology Center.<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Organization<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"TRW Inc. Materials and Manufacturing Technology Center.<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/viaf.org\/viaf\/155061179<\/a>> # Lewis Research Center.<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Organization<\/a> ;\u00A0\u00A0\u00A0schema:name<\/a> \"Lewis Research Center.<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/viaf.org\/viaf\/23544921<\/a>> # Donald J. Moracz<\/span>\u00A0\u00A0\u00A0\u00A0a schema:Person<\/a> ;\u00A0\u00A0\u00A0schema:familyName<\/a> \"Moracz<\/span>\" ;\u00A0\u00A0\u00A0schema:givenName<\/a> \"Donald J.<\/span>\" ;\u00A0\u00A0\u00A0schema:givenName<\/a> \"D. J.<\/span>\" ;\u00A0\u00A0\u00A0schema:name<\/a> \"Donald J. Moracz<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/www.worldcat.org\/title\/-\/oclc\/11674423<\/a>>\u00A0\u00A0\u00A0\u00A0a genont:InformationResource<\/a>, genont:ContentTypeGenericResource<\/a> ;\u00A0\u00A0\u00A0schema:about<\/a> <http:\/\/www.worldcat.org\/oclc\/11674423<\/a>> ; # Fabrication development for ODS-superalloy, air-cooled turbine blades : final report<\/span>\u00A0\u00A0\u00A0schema:dateModified<\/a> \"2018-11-11<\/span>\" ;\u00A0\u00A0\u00A0void:inDataset<\/a> <http:\/\/purl.oclc.org\/dataset\/WorldCat<\/a>> ;\u00A0\u00A0\u00A0\u00A0.<\/div>
<http:\/\/www.worldcat.org\/title\/-\/oclc\/11674423#PublicationEvent\/cleveland_ohio_national_aeronautics_and_space_administration_nasa_lewis_research_center_springfield_va_for_sale_by_the_national_technical_information_service_1984<\/a>>\u00A0\u00A0\u00A0\u00A0a schema:PublicationEvent<\/a> ;\u00A0\u00A0\u00A0schema:location<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Place\/springfield_va<\/a>> ; # Springfield, Va.<\/span>\u00A0\u00A0\u00A0schema:location<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Place\/cleveland_ohio<\/a>> ; # Cleveland, Ohio?<\/span>\u00A0\u00A0\u00A0schema:organizer<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Agent\/for_sale_by_the_national_technical_information_service<\/a>> ; # [For sale by the National Technical Information Service]<\/span>\u00A0\u00A0\u00A0schema:organizer<\/a> <http:\/\/experiment.worldcat.org\/entity\/work\/data\/4482037#Agent\/national_aeronautics_and_space_administration_nasa_lewis_research_center<\/a>> ; # National Aeronautics and Space Administration, NASA Lewis Research Center<\/span>\u00A0\u00A0\u00A0schema:startDate<\/a> \"1984<\/span>\" ;\u00A0\u00A0\u00A0\u00A0.<\/div>

Content-negotiable representations<\/p>